ASME SB111 C68700 Seamless Brass Tubes for Desalination of Seawater
C68700 is an aluminum brass alloy with arsenic addition, specifically designed for harsh environments such as seawater desalination. Its composition (Cu: 76-79%, Al: 1.8-2.5%, As: 0.02-0.06%, Zn: balance) ensures exceptional corrosion resistance in seawater and high thermal conductivity. The arsenic content further enhances resistance to dezincification, a critical feature for long-term durability in marine applications.
The production process of Brass Tube
Raw Materials
Melting&Casting
Extrusion
Rolling
Intermediate Heat Treatment 1
Straightening
Three-line Drawing
Acid Washing
Intermediate Heat Treatment 2
Two Cascade Drawing
Cutting&Cleaning
Eddy Current Test
Final Heat Treatment
Packing
Shipping
Comparison Table of Brass Tube Alloy
Implementation Standard | Alloy Specifications |
GB/T 5231 | HAI 77-2 |
HSn70-1, HSn72-1 | |
ASTM B111 | C68700 |
C44300 | |
BS EN12451 | CuZn20Al2As |
CuZn28Sn1As | |
JIS H3300 | C6870, C6871, C6872 |
C44300 | |
AS 1569 | C68700 |
C44300 |
Chemical Composition of Brass Tube Alloys
Implementation Standard | Alloy | Cu (%) | Al/Sn (%) | As (%) | Fe (%) | Pb (%) | Other Impurities (%) | Zn (%) | Total Impurities (%) |
GB/T 5231 | HAl77-2 | 76.0-79.0 | 1.8-2.5 (Al) | 0.02-0.06 | ≤0.06 | ≤0.07 | ≤0.07 (Other) | Balance | ≤0.6 |
ASTM B111 | C68700 | 76.0-79.0 | 1.8-2.5 (Al) | 0.02-0.06 | ≤0.06 | ≤0.07 | ≤0.07 (Other) | Balance | ≥99.5 (Sum) |
ASME SB111 | |||||||||
JIS H3300 | C6870 | 76.0-79.0 | 1.8-2.5 (Al) | 0.02-0.06 | ≤0.05 | ≤0.05 | ≤0.05 (Other) | Balance | - |
JIS H3300 | C6871 | 76.0-79.0 | 1.8-2.5 (Al) | 0.02-0.06 | ≤0.05 | ≤0.05 | ≤0.05 (Other); Si: 0.20-0.50 | Balance | - |
JIS H3300 | C6872 | 76.0-79.0 | 1.8-2.5 (Al) | 0.02-0.06 | ≤0.05 | ≤0.05 | ≤0.05 (Other); Ni: 0.20-1.0 | Balance | - |
BS EN12451 | CuZn20Al2As (CW702R) | 76.0-79.0 | 1.8-2.3 (Al) | 0.02-0.06 | ≤0.07 | ≤0.05 | Ni ≤0.1; P ≤0.01; Mn ≤0.1; ≤0.3 (Other total) | Balance | - |
AS 1569 | C68700 | 76.0-79.0 | 1.8-2.5 (Al) | 0.02-0.06 | ≤0.06 | ≤0.07 | ≤0.07 (Other) | Balance | - |
GB/T 5231 | HSn70-1 | 69.0-71.0 | 0.8-1.3 (Sn) | 0.03-0.06 | ≤0.10 | ≤0.05 | ≤0.05 (Other) | Balance | ≤0.3 |
GB/T 5231 | HSn72-1 | 70.0-73.0 | 0.9-1.2 (Sn) | 0.02-0.06 | ≤0.06 | ≤0.07 | ≤0.07 (Other) | Balance | ≤0.4 |
ASTM B111 | C44300 | 70.0-73.0 | 0.9-1.2 (Sn) | 0.02-0.06 | ≤0.06 | ≤0.07 | ≤0.07 (Other) | Balance | ≥99.6 (Sum) |
ASME SB111 | |||||||||
JIS H3300 | C4430 | 70.0-73.0 | 0.9-1.2 (Sn) | 0.02-0.06 | ≤0.05 | ≤0.05 | ≤0.05 (Other) | Balance | - |
BS EN12451 | CuZn28Sn1As (CW706R) | 70.0-72.5 | 0.9-1.3 (Sn) | 0.02-0.06 | ≤0.07 | ≤0.05 | Ni ≤0.1; P ≤0.01; Mn ≤0.1; ≤0.3 (Other total) | Balance | - |
AS 1569 | C44300 | 70.0-73.0 | 0.8-1.2 (Sn) | 0.02-0.06 | ≤0.06 | ≤0.07 | ≤0.07 (Other) |
|
Primary Applications in Seawater Desalination
Heat Exchangers and Condensers
Corrosion Resistance
Mechanical Performance